====== Bees Wax ====== ===== Cleaning ===== - hold part with pliers - heat up with very hot water - Wipe off with paper towel - Clean threads with a toothpick or a metal pin ===== Settings / profiles ===== * 1,6w 0,2z 15f 0pct * 3D object: Cone * 35°C filament, no fan, no bed * --> FAIL * 1,6w 0,4z 7f 0pct * 3D object: Cone * 35°C filament, no fan, no bed * --> Filament stopped adhering to print bed after a while * No random layer restarts * Higher layer height * much more flow * First layers are okay, Adhesion only occurs on motor override * 1,6w 0,8z 7f 0pct * 35°C filament, no fan, no bed * OK: first layer sticks with uhu-glue * After ±3 layers: material doesn't want to stick onto itself. * --> Increase extrusion width from 1.7 to 2.2 (future me: extrusion width doesn't change material flow. It just changes the distance between lines) * --> Layer height 1mm everywhere * Beeswax 01 * 35°C filament, no fan, no bed * Using Uhu-glue * There are gaps between lines * not enough extrusion 17/04/2019 3D model: cone * Beeswax 01 (0,8z 7f) * nozzle: 35°C * bed: 25°C * result: Prints beautifully. Z-axis skipping (Z-axis motion is too fast). Layers delaminate easily, as they are not fused. * Beeswax 01 * nozzle: **40°C** * bed: 25°C * result: same as above * Beeswax 01 * nozzle **45°C** * bed: 25°C * result: flakey / grainy texture, but stronger layer adhesion. * Beeswax 01 * nozzle: **50°C** * bed: 25°C * result: super flakey * Beeswax 01 * nozzle: 50°C * bed: 25°C * **warm up time: 15min** * result: a little more consistent * Beeswax 01 * nozzle: 50°C * bed: 25°C * warm up time: **40min** * result: same as above * Beeswax 01 * nozzle: **55°C** * bed: 25°C * warm up time: **30min** * result: separated material: half oil, half solid. 3D print has a dripped texture. The tip of the syringe is cooler. The body of the syringe is much hotter. * Beeswax 02 (1w 0,5z 7f) * nozzle: **60°C** * bed: 25°C * warm up time: **50min** * result: Almost completely liquid. Too liquid for the nozzle width. * Beeswax 03 (1w **0,15z** 7f) * nozzle: **60°C** * bed: 25°C * result: Still a little smudgy. Good consistency: creates homogenous lines. 24/04/2019 * Beeswax 4 (0,6w 0,15z 7f) * filament: 70°C * shape: cone * result: a luer tip with 0,6mm inner diameter cools the wax down too much, resulting in jams and sudden eruptions of hot wax. *Beeswax 4 (1,18w 0,15z 7f) * filament: 70°C * shape: cone * result: OK, but printing too slow: cools down too fast *Beeswax 4 (1,18w 0,15z **20f**) * filament: 70°C * shape: cone * result: Material flow stops. There is a weird buzz which I think is an unprime event. *Beeswax 4 (1,18w 0,15z 20f) * filament: 70°C * shape: cone * **head control**: unprime set to zero * result:? * Beeswax 5 * filament: 35°C * shape: vessel v1 * result: layers too thick, had to change material flow rate multiplier to 1.5.