Differences
This shows you the differences between two versions of the page.
Both sides previous revisionPrevious revisionNext revision | Previous revisionNext revisionBoth sides next revision | ||
3devo_extruder:3devo_extruder [2019/08/07 07:24] – [Shutting down] formlab | 3devo_extruder:3devo_extruder [2020/06/16 06:23] – [Hydrate filament] formlab | ||
---|---|---|---|
Line 25: | Line 25: | ||
+ | ===== Dry filament ===== | ||
+ | * 4-6 hours @70-80°C. | ||
+ | * Other sources say to stay below 40°C | ||
+ | |||
+ | |||
+ | |||
===== Hydrate filament ===== | ===== Hydrate filament ===== | ||
* When the filament is too brittle | * When the filament is too brittle |