Table of Contents

Formech 1372

Thermoform machine

Forming area

Plastic sheet sizes

Pre-drying

Vacuum Forming Guide


Mould tips

Moulds should not contain moisture or dust (!) since it could harm the vacuum pump.

Tested mould materials include:

Available sheet materials

PETG - Polyethylene terephthalate glycol-modified

Transparent, glossy surface.

Thickness Size Cost (per sheet)
1mm Large - 1370 x 660mm €16,10
2mm Large - 1370 x 660mm €32,20
1mm Small - 500 x 500mm €4,20
2mm Small - 500 x 500mm €7,14
3mm Small - 500 x 500mm €10,36


PMMA samples

PMMA - Poly(methyl methacrylate)

PMMA is also known as Acryl. It has a glossy surface.

Color Light Thickness Size Cost (per sheet)
White translucent 3mm large - 1370 x 660mm €39,20
White translucent 3mm small - 500 x 500mm €11,20
Green transparent 3mm small - 500 x 500mm €16,80
Light blue translucent 3mm large - 1370 x 660mm €58,80
Light blue translucent 3mm small - 500 x 500mm €16,80
Dark blue transparent 3mm large - 1370 x 660mm €58,80
Dark blue transparent 3mm small - 500 x 500mm €16,80
Yellow transparent 3mm small - 500 x 500mm €16,80
Cream transparent 3mm large - 1370 x 660mm €58,80
Cream transparent 3mm small - 500 x 500mm €16,80


polystyrene samples

PS - Polystyrene

Uncut sheets. These can be used for the large and small forming area.

Color Surface finish Thickness Size Cost (per sheet)
white matte / glossy 1mm 2000×1200 €19,63
white matte / glossy 1,5mm 2000×1200 €28,88
white matte / matte 4mm 2000×1000 €63,42
black matte / matte 1mm 2000×1200 €22,06
black matte / glossy 1,5mm 2000×1200 €35,19
red matte / matte 1mm 2000×1200 €22,06
red matte / glossy 1,5mm 2000×1200 €35,19
green matte / matte 1,5mm 2000×1200 €34,03

How much does it cost?

startup cost + ( plastic sheet cost * plastic sheet count * material multiplier )
+
( machine time (minutes) * machine time cost )

Materials allowed in Formlab

HIPS - high impact polystyrene

PETG - Polyethylene terephthalate glycol-modified

HDPE - High density polyethylene

PP - polypropylene


Materials NOT allowed in Formlab

ABS - Acrylonitrile butadiene styrene

PC - polycarbonate

PVC - polyvinyl chloride

PMMA - Poly(methyl methacrylate)

PET - Polyethylene terephthalate

General tips

Drying sheets with the oven

Use one of the ceramics oven in the metal atelier.
The control cabinet is behind the oven.

Get the key from Peter to be able to power on the oven.
To turn on the oven, insert the key and turn it to the right. Then turn the red knob to the right.

Control panel

  1. Press 'program' until it goes to program 5
    1. Nothing is on here yet. (This might change in the future)
    2. Press until there's an empty preset
    3. In the future there might be a paper with an explanation of what programs do what. I could have a fixed entry on the list
  2. Segment 1' is blinking. Use the up-down arrows to set a target temperature
  3. Press the –> arrow to go to the time value
  4. Set the time with the up-down arrows
  5. When ready, press the stop / start button to start the oven

Suggested program

Clamping tips for high gauge sheets

Machine presets

PS

PETG

PMMA

Medium Gauge Film

—-

Troubleshooting

Preset loading gives wrong values

Reason of problem: touch screen input is too fast for the slow computer (PLC)

Fix:

Sheet pulls itself out of the clamping frame

Formech: The material is presumably not reaching the correct forming temperature, so the sheet is far stiffer than it should be, making it hard to pre-stretch the material and also as the tool comes up on the table the inflexibility of the material requires much more clamping force on the clamp frame. This is why the sheet is pulling out. If you are using the full forming aperture then you will have better clamping, providing your machine has the 8mm round silicone bead seal as shown below.


If you are using a reducing window, then you will have to make sure that you have good clamping on each side of the aperture. The reducing window seals are flat silicone sponge and do not have the same gripping effect as the round silicone bead seal.


Formech: You could also try turning over the sheet several times during heating to try and replicate a double heater machine, so that the heat penetrates the sheet from both sides. Formlab: this method doesn't work easily on big sheets since it sags and becomes flexible. It's not easy to clamp again in the frame. Polycarbonate loses moest heat in the process.

Blisters appear on the surface

There is moisture in the sheet. At the point the blisters appear, the sheet is not hot enough to form yet. You'll need to dry the sheet or switch to a non hygroscopic material.

Pre-stretch button does nothing

Heater timer doesn't count down